ABSTRACTThis article describes several experiments conducted on single lap joints (SLJ) subjected to tensile mechanical loads. Two epoxy adhesives, with slow and fast curing, were used, with a weight of 0%, 3%, and 10% of glass microspheres and milled glass particles, respectively. The adherends used in the construction of the specimens were fiber-reinforced polymers. The types of failures produced in the SLJ specimens were classified according to ASTM standards. The results of the experimental tests on the SLJ with fast-curing epoxy adhesive showed that the use of milled glass and glass microspheres improved the strength of the joint compared with the neat fast-curing epoxy adhesive. As for the experimental test on the joint with slow-curing epoxy adhesive, the results showed that the use of milled glass and glass microspheres decreased its strength when using different additive concentrations compared with the neat slow-curing epoxy adhesive.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.