In this research paper, drinking water was used as dielectric fluid and Ti-6Al-4V alloy was machined on EDM. The process parameters were discharge current, pulse on time, pulse off time and graphite powder concentration. The graphite powder concentration was 4.5 g/l, 9 g/l and 13.5 g/l were mixed in drinking water. Experiments were carried out based on Taguchi L27 orthogonal array. Individual significant process parameters were evaluated by the analysis of variance (ANOVA). The material removal rate, surface roughness and recast layer thickness were optimized by Taguchi methodology. The maximum material removal rate was 10.567 mm3/min at 4.5 g/l. The low surface roughness was 2.31 µm and recast layer thickness was 8.42 µm both were found at 9 g/l. EDAX Analysis and micro hardness test were also carried out.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.