Abstract

The objective of the presented investigation was to verify findings that moisture has a negative effect on the bond force leading to a reduction of the mean maximum shear force up to 30% for long term water storage or combined pressure and short term water storage at 40°C. Additionally, the influence on maximum shear stiffness was investigated. Furthermore, it was assumed that the reduction of shear properties would increase with higher applied temperature. The investigation was conducted using different up to date pavement structures for urban roads and heavy trafficked motorways. The chosen material represents the actual Swiss construction practice favoring relatively open graded low noise surface courses. Testing was done using the Layer-Parallel Direct Shear device (LPDS) and the Shear Box as an additional measure for the shear properties. The results showed that 72h water conditioning at 40°C reduces interlayer shear strength by 2% to 20%. 72h water conditioning at 60°C is more severe, reducing strength by 15% to 25% and stiffness by 14% to 30%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.