Abstract

The development of a porous free zone of the silicon cemented layer represents a scientific and technical challenge. The limitation of the effects of the Kirkendall–Frenkel phenomena requires the right control of the thermochemical processing parameters (temperature, time, and chemical) and thorough knowledge of the related interaction with the specific elements of the metallic matrix of the thermochemically processed product. Through the experimental programming method, the individual and cumulated effects of the thermochemical processing parameters on (Fe-Armco) high-purity iron cemented by silicon in ferrosilicon (FeSi75C) powdered solid media have been quantified. It was concluded that ferrosilicon with silicon concentrations higher than 60% (FeSi75C) represents a redoubtable active component, especially in a temperature range higher than 1100 °C. In the layer cemented with silicon, the presence of nitrogen was also observed, as a direct consequence of the composition of the medium used for cementation. The presence of this element is the predominant result of the manifestation of the ionic phenomenon of adsorption. The correlations between these parameters and the dimension of the porous free zone of the silicon cemented layer in the vicinity of the thermochemically processed surface have been determined.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.