To increase the limiting drawing ratio (LDR) in deep drawing, experiments are conducted on DP600, IF, and HSLA steels. The flange region of blank is heated up to temperatures in the warm range by inductance heating. During heating, the central portion of blank is cooled by water to prevent the reduction of the strength of the material in the central region. The temperature increase of flange region is observed by two infrared sensors focusing on two different points, one on the blank rim and the other near the die radius. An intensive cooling by cold water is applied to the bottom side of a blank during deep drawing. Increases up to 25.58% on LDR are obtained. There is no significant change in the microstructure of the material due to warm forming. Material characterization is obtained by a Gleeble 3800 thermo-mechanical testing machine for the temperature range 150–300 °C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.