We present real-time observations of the directional-solidification patterns of a transparent nonfaceted eutectic alloy (CBr4-C2Cl6) in bulk samples. The growth front of the two-phase solid is observed from the top through the liquid and the glass wall of the container with a long-distance microscope. We show that, in near-eutectic CBr4-C2Cl6 alloys, the upper stability limit of the stationary lamellar patterns is due to a zigzag bifurcation, which occurs at an interlamellar spacing of about 0.85 lambda(m), where lambda(m) is the minimum-undercooling spacing. The zigzag patterns undergo a lamella breakup instability leading to the creation of new lamellae at about 1.1 lambda(m). On the other hand, the lower stability limit of the stationary patterns is due to the same instability as in thin samples, namely, a lamella termination instability that occurs at about 0.7 lambda(m).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.