Abstract

In the present study, six silicone rubber doped by tellurium borate oxides were fabricated using the casting method. The densities of the fabricated silicon rubber-doped by tellurium borate oxides samples were measured using the Archimedes Method. Moreover, the linear attenuation coefficient of silicone rubber doped tellurium borate oxides samples was evaluated experimentally using the hyper pure germanium, and the recorded linear attenuation coefficient values were affirmed using the theoretical Phy-X program. The experimental measurements were performed using the narrow beam transmission method with radioactive isotopes Am-241, Cs-137, and Co-60 with energies of 59, 661, 1173, and 1332 keV. The linear attenuation coefficient values showed an enhancement by 4.73 times, 1.20 time, 1.17, time, and 1.17 time, respectively at gamma photon energies of 59, 661, 1173, and 1332 keV, when the TeO2 concentration increased in the fabricated composites from 0 to 50 wt%. The enhancement of the linear attenuation coefficient values has a positive effect on the transmission rate values where the half-value thickness and transmission rate were decreased accompanied by an increase in the RPE.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.