Abstract
The paper outlines the results of an investigation to characterize the response of P75/934 graphite/epoxy tubes with a stacking sequence of [15/0/±10/0/−15] s under pure torsion and combined axial/torsion loading. The experimentally observed nonlinear response and path-dependent failure are discussed in terms of material nonlinearities at the ply level and first-ply failure loads with the help of an analytical model.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.