Abstract

In the present paper, the meaning of an isoclinic parameter appearing in the elasto-visco-plastic state of a transparent material is investigated experimentally.Celluloid softened by heating is selected as the elasto-visco-plastic material. A complex loading having a trajectory which consists of two branches intersecting normally is realized on a thin-walled cylindrical shell of celluloid heated at 65°C with the sequences of axial tension and torsion.The relation between isoclinic parameter and the directions of principal stress and principal strain is investigated on the trajectory after its corner in relating the amount of pre-strain.As the result of experiment, the following trends may be concluded. After the rotation of principal axis of stress with a large difference between the principal stress and strain differences, though the isoclinic parameter shows the direction of principal stress for the pre-strain less than a certain value, it tends to the direction of principal strain from that of principal stress with an increase of strain after the corner for a pre-strain larger than that value.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.