Exchange current density (i∘) of thorium in LiCl-KCl eutectic at tungsten(inert) and liquid cadmium electrodes is reported in the present work. A cadmium electrode was designed in our laboratory for estimating i∘ of thorium in liquid cadmium. Cyclic voltammetry of thorium at tungsten electrode was associated with a cathodic peak at −1.59V at 773K attributed to Th4+|Th redox couple. Cathodic peaks corresponding to Th4+|ThCd11 and Th4+|ThCd5 couples at −1.31V and −1.38V, respectively (at 773K) were observed in the cyclic voltammograms of thorium at liquid cadmium electrode. i∘ of thorium in LiCl-KCl eutectic at tungsten electrode (cathodic polarization) estimated by Tafel and Allen-Hickling methods were compared with those estimated from the cyclic voltammograms of LiCl-KCl-ThCl4. i∘ at tungsten electrode was found to be higher than that at liquid cadmium electrode. The temperature dependence of i∘ was studied to estimate the activation energy associated with Th4+|Th couple at tungsten, liquid cadmium (cathodic polarization) and dissolution of thorium (anodic polarization). The compositional dependence of i∘ of thorium at tungsten electrode was also addressed. This is the first report on the i∘ of thorium in LiCl-KCl eutectic.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.