Abstract

In this paper, the influence of two selected parameters (the welding time and the presence of the activating flux on the surface of the base metal) on the weld joint at Stud Arc Welding process is investigated. In the experimental part of the paper, the drawn arc stud welding process with the ceramic ferrule is applied with the different welding time and the application of the activating flux for ATIG process. In order to evaluate the influence of the welding time and the activating flux on the weld characteristics, the cast zone width and Vickers hardness HV 0.2 are measured.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.