Abstract

The microstructure of α-brass has been investigated at 98% and 200% of cryorolling (CR). Severe cryorolling introduces microscopic shear bands, forms primary and secondary twins, and the twin density increases with increase of plastic strain. Even though the average hardness values in CR200 (197 Hv) does not increase significantly than that of CR98 (189 Hv), but the hardness distribution become narrow in CR200 due to the narrow size distribution and refinement of twin lamellar spacing. The microscopic mechanism on the evolution of homogeneous nanostructure in α-brass has been reported.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.