Abstract

This paper investigated the microstructure, tensile properties, intergranular corrosion resistance and exfoliation corrosion resistance of Al-4.5Zn-1.5Mg (wt.%) alloy after undergoing different numbers of flame rectification at 350°C. The results showed that in the flame correction area, the mechanical properties of Al-4.5Zn-1.5Mg(wt.%) alloy with two times of flame correction is the best. The maximum tensile strength and elongation of Al-4.5Zn-1.5Mg(wt.%) alloy inside the region of flame correction are 387MPa and 26.37% respectively. The flame rectification accelerated the corrosion susceptibility of Al-4.5Zn-1.5Mg (wt.%) alloy. The maximum intergranular corrosion depth is detected with the value of 105μm after one time of FR. The corrosion property of Al-4.5Zn-1.5Mg(wt.%) alloy is mainly related to the formation of galvanic couple. The uneven distribution of the second phase particles of Al-4.5Zn-1.5Mg(wt.%) alloys results in different corrosion potentials at grain boundaries and within grains, leading to galvanic corrosion.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.