Nanocrystals, with a body-centered-cubic crystal structure of lattice parameter 18.2525 Å , were found in amorphous Pd40.5Ni40.5P19 specimens that had been annealed at 628 K for 30 min. The crystal surfaces are smooth and dislocations are absent, suggesting that the growth of these nanocrystals is through a two-dimensional nucleation and growth mechanism (formation of surface nuclei of critical size and their subsequent growth).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.