Abstract
The low-temperature crystal structure of elemental lithium, the prototypical simple metal, is a several-decades-old problem. At 1 atm pressure and 298 K, Li forms a body-centered cubic lattice, which is common to all alkali metals. However, a low-temperature phase transition was experimentally detected to a structure initially identified as having the 9R stacking. This structure, proposed by Overhauser in 1984, has been questioned repeatedly but has not been confirmed. Here we present a theoretical analysis of the Fermi surface of lithium in several relevant structures. We demonstrate that experimental measurements of the Fermi surface based on the de Haas-van Alphen effect can be used as a diagnostic method to investigate the low-temperature phase diagram of lithium. This approach may overcome the limitations of X-ray and neutron diffraction techniques and makes possible, in principle, the determination of the lithium low-temperature structure (and that of other metals) at both ambient and high pressure. The theoretical results are compared with existing low-temperature ambient pressure experimental data, which are shown to be inconsistent with a 9R phase for the low-temperature structure of lithium.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have