Abstract

Evaporation of Pb and Li from molten Pb17Li was investigated between 350 and 800°C in vacuum, argon and helium covergas. Results were also obtained from other experimental facilities. Similarities were found to observations from sodium cooled reactors. The results show that Pb and Li evaporate independent on each other. The two elements show different behavior along the transport pathway. Deposits of the evaporated metals contained between 0.2 and 98 at% Li. As in the reactor RAPSODIE for sodium, evaporation rates for lithium were smaller in helium than in argon, however evaporation rates of lead were the same in both gases. No aerosol problems will exists with normal blanket operation. Under experimental conditions, aerosol concentrations were in the range of 10 −9 to 10 −6 g/m 3. Aerosols can easily be trapped with sintered metal filters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.