The level of internal stresses arising in the titanium VT1-0 + steel 08kp bimetal during cooling was estimated by methods of finite element modeling. It is shown that the intermetallic layer formed during diffusion annealing leads to a sharp local increase in the residual internal equivalent Mises stresses with a slight decrease in the stresses normal to the interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.