Abstract

Residual performance of old architectural wood which has been damaged was measured using Nondestructive Evaluation (NDE). The wood Pole Tester was used to assess ultrasonic velocity inside wood and drill resistance was determined using an IML-resistograph. For ultrasonic measurements squared timber and circular timber`s measurements were separately conducted with 1,300 m/s as the standard ultrasonic velocity. The standard wood samples divided into two parts; a non-sound area (below the standard), and a sound area (above the standard). Furthermore, schematization of wood was compared with results naked eye observation. The drilling resistance test was performed for both length and thickness direction in wood. The internal of the drilling was set at 30 cm (length direction), 5 cm (width direction) and 30cm (thickness direction). A non-sound area was defined as that 1) amplitude is below 20% and 2) carbonization and deterioration are related.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call