Abstract

The aim of this study was to evaluate the level of residual monomer in acrylic denture base materials having different polymerization properties. The investigation included a conventional-type acrylic cured under heat and pressure, as well as a pour-type resin polymerized by an injection-moulding technique at room temperature and under pressure. It was found that the residual monomer content ranged from 0.22-0.54% in pour-type resin, and from 0.23-0.52% in routinely used resins when the specimens were analysed by high performance liquid chromatography. These findings revealed that there were no significant differences between the two types of acrylic in terms of their residual monomer content.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.