Abstract

To avoid geometrical inefficiencies in the ATLAS pixel detector, the concept of shingling is used up to now in the barrel section. For the upgrades of ATLAS, it is desired to avoid this as it increases the volume and material budget of the pixel layers and complicates the cooling. A direct planar edge-to-edge arrangement of pixel modules has not been possible in the past due to about 1100 μ m of inactive edge composed of approximately 600 μ m of guard rings and 500 μ m of safety margin. In this work, the safety margin and guard rings of ATLAS SingleChip sensors were cut at different positions using a standard diamond dicing saw and irradiated afterwards to explore the breakdown behaviour and the leakage current development. It is found that the inactive edge can be reduced to about 400 μ m of guard rings with almost no reduction in pre-irradiation testability and leakage current performance. This is in particular important for the insertable b-layer upgrade of ATLAS (IBL) where inactive edges of less than 450 μ m width are required.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.