Abstract

Mechanical behaviour of unsaturated polyester resin reinforced with foundry slag is used for the composite materials has been studied to determine various important parameters, such as tensile and flexural properties by using moulding process. 75 µm level particle sizes of fine powdered foundry slag are used for sample preparation. Concentration of powdered slag is varied from 5%, 7.5%, 15% by weight in the polyester resin. The composite test specimens are prepared using moulding process as per ASTM D638 for tensile test and ASTM D 790 for Flexural test.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.