Temporal changes in the number density, size distribution, and chemical composition of clusters formed during natural aging at room temperature and pre-aging at 363 K (90 °C) in an Al-0.62Mg-0.93Si (mass pct) alloy were evaluated using atom probe tomography. More than 10 million atoms were examined in the cluster analysis, in which about 1000 clusters were obtained for each material after various aging treatments. The statistically proven records show that both number density and the average radius of clusters in pre-aged materials are larger than in naturally aged materials. It was revealed that the fraction of clusters with a low Mg/Si ratio after natural aging for a short time is higher than with other aging treatments, regardless of cluster size. This indicates that Si-rich clusters form more easily after short-period natural aging, and that Mg atoms can diffuse into the clusters or possibly form another type of Mg-Si cluster after prolonged natural aging. The formation of large clusters with a uniform Mg/Si ratio is encouraged by pre-aging. It can be concluded that an increase of small clusters with various Mg/Si ratios does not promote the bake-hardening (BH) response, whereas large clusters with a uniform Mg/Si ratio play an important role in hardening during the BH treatment at 443 K (170 °C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call