Abstract
Residual creep life evaluation is an essential part of Fitness-For-Service (FFS) assessment for engineering components operating at elevated temperatures. This paper elaborates a new evaluation approach based on macro-pillar compression testing (MPCT) and Omega method. The MPCT creep test was performed at the same stress level as the tensile creep test by adjusting the testing load using an algorithm, which is also provided in this paper. The barreling effect of MPCT creep test was corrected by two proposed parameters, which were calibrated using finite element method with 6 types of Cr-Mo alloys from API 579. Finally, a 1.25Cr-0.5Mo-Si steel was prepared for both MPCT and round bar tensile creep tests at 550 ℃ and different initial stress levels. The predicted residual creep life by MPCT has an error of 2.2% at 140 MPa, 6.4% at 160 MPa and 13.5% at 180 MPa.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.