AbstractComposite resins represent a class of material widely used in restorative dentistry, not only for anterior aesthetics but also as the first choice to restore posterior teeth. However the key limitation in the use of composite resins as a restorative material is related to shrinkage during polymerization which leads to poor marginal seal, marginal staining, restoration displacement, tooth fracture and recurring caries [1].Polymerization shrinkage may affect negatively the clinical outcome of the restoration. Hence the present study evaluates the Polymerization shrinkage of 2 different posterior composites; Filtek Z350(3M) and everX Posterior(GC), using a pycnometer.Independent Sample T-Test was used to determine statistically significant difference in volumetric shrinkage among the tested composite resins. everX Posterior showed comparatively less shrinkage than Filtek Z350; which can be attributed to the presence of silanated e-glass fibres.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.