Abstract

Si 3N 4 (SN-281)/Cu-clad-Mo joints, brazed using a soft (YS: 341 MPa) and ductile (43% elongation) Pd–Co braze were sound and exhibited an interaction zone comprised of Pd 66Mo 14Cu 10Co 6Si 3 and Pd 74Mo 11Co 8Cu 6Si. Similar joints made using a less ductile and stronger Pd–Ni braze led to cracking from large CTE mismatch-induced strain energy (∼64 mJ to 348 mJ).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.