Abstract
In this study, 6061-T6 aluminum alloys were plated with electroless Ni-P with different phosphorus content and three-point bending and rotary bending fatigue tests. The effects of hydrogen due to plating on mechanical properties were investigated. It was shown that the ductility decreased immediately after low-phosphorus type and high-phosphorus type Ni-P plating by three-point bending test because a hydrogen was introduced into the alloys. The fatigue strength of the low-phosphorus type Ni-P plated specimen was higher than that of the untreated specimen, while that of the high-phosphorus type plated specimen was much lower. It is clear that the fatigue strength differs greatly depending on the phosphorus content in the plating film. 6061-T6 aluminum alloy have been reported to exhibit no hydrogen embrittlement in low strain rate tensile tests under wet condition. However, it was found that hydrogen embrittlement occurred when 6061-T6 aluminum alloy was plated with the high-phosphorus type electroless Ni-P and fatigue-tested on rotary bending machine.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Institute of Metals and Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.