ObjectiveThe aim of this study was to compare the effects of different enamel conditioning techniques for bracket bonding.MethodsNinety-one human premolars were randomly divided in six groups of 15 specimens each. The enamel surfaces of the teeth were etched with 35% orthophosphoric acid in Group 1, with a self-etching primer in Group 2, sandblasted in Group 3, sandblasted and etched with 35% orthophosphoric acid in Group 4, conditioned by Er:YAG laser in Group 5 and conditioned by Er:YAG laser and etched with 35% phosphoric acid gel respectively in Group 6. After enamel conditioning procedures, brackets were bonded and shear bonding test was performed. After debonding, adhesive remnant index scores were calculated for all groups. One tooth from each group were inspected by scanning electron microscope for evaluating the enamel surface characteristics.ResultsThe laser and acid etched group showed the highest mean shear bond strength (SBS) value (13.61 ± 1.14 MPa) while sandblasted group yielded the lowest value (3.12 ± 0.61 MPa).ConclusionsAlthough the SBS values were higher, the teeth in laser conditioned groups were highly damaged. Therefore, acid etching and self-etching techniques were found to be safer for orthodontic bracket bonding. Sandblasting method was found to generate inadequate bonding strength.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.