Abstract

Introduction: The aim of this study was the Evaluation of compressive strength and setting expansion of GC and Adenta dye stones. Materials & Methods: This study was an experimental study. The sample number was 21 for each group (n = 21). Compressive strength and setting expansion of GC and Adenta dye stones was tested based on ADA Standard 25 and Iranian Standard No. 2792. Data analysis was done with Independent-Sample t-test (p value = 0.05). Results: There was no significant difference between GC (47.61 ± 5.54) and Adenta groups (44.31 ± 7.71) in terms of compressive strength. Also, there was no significant difference in the setting expansion between GC (0.07 ± 0.008) and Adenta dye stones (0.08 ± 0.001). Conclusion: The results of this study showed that there is no statistically significant difference in setting expansion and compressive strength between GC and Adenta dye stones and both samples was under standard condition )p value < 0.05).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.