Abstract

The O-rings in ball retained overdentures deteriorate with time and need replacement to restore the retentive quality. We evaluated retrospectively the mechanical properties of O-rings after 3 years in function in 1 and 2-piece implant-supported overdentures. The O-rings were retrieved from one-piece (Myriad snap, Equinox-Straumann, 3.3 × 13 mm) and 2-piece (Neo Biotech, 3.3 × 13 mm) implant-supported overdenture patients. A total of 16 pairs of matrices were tested for wear, type of damage, and elasticity using Pin on Disc method, USB Digital Camera in 30× zoom and Universal Tensile Machine, respectively. The statistical analysis for independent groups were done with the Mann-Whitney U test. Assessment of used O-rings showed 84% more wear in the 2-piece system with an abrasive type of damage while 46% wear in the 1-piece system with a compressive type of damage. The O-rings in 1-piece system showed increase in elongation and maximum displacement to 2% and 7%, respectively, whereas the 2-piece system showed decrease in elongation and maximum displacement by 13% and 6%, respectively. In 1-piece system, the loss of retention was more with slow wear rate, and in 2-piece system, the wear resistance of O-rings decreased due to increased stiffness. Further studies to evaluate the changes in O-ring with increased sample size and at interval 1 year will pave way for insight into the progressive changes in the mechanical properties of an O-ring.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call