Abstract

Accelerated shotcrete is a common method of ground support used in underground mines in Australia. Sufficient early strength gain relies upon the chemical composition of the shotcrete accelerator and the cement with which it reacts. The chemical composition of Ordinary Portland Cement used in shotcrete application varies significantly throughout Australia. Early strength development after the application of shotcrete is a determining factor for calculating the re-entry time during in-cycle underground mining. Due to the variance in the cement chemistry available in Australia, this article will show the effect of different cement on early strength development. Analysis of the most commonly used cements in Australia will be shown and how they can be classified. An overview of the cement chemistry of Australian cements and the impact of the cement chemistry on the early strength development using a set of standard shotcrete accelerators will be shown. The objective of this paper is to provide inside information to geotechnical engineers on the reaction time difference between different cements and standard shotcrete accelerators. This research is expected to provide greater confidence to geotechnical engineers in trouble shooting shotcrete early strength problems.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.