Abstract

AbstractThe objective of the present study is to determine the threshold stress level of stress corrosion cracking (SCC) in AA7075-T651 aluminium alloy by suitable experimentation. The test was carried out using a circumferential notch specimen in a horizontal-type constant load SCC setup in a 3.5 wt.% NaCl solution. The time to failure by SCC was determined at various loading conditions. The threshold stress of AA7075-T651 alloy was found to be 242 MPa in a 3.5 wt.% NaCl solution. The various regions of the fractured surface specimen such as machined notch, SCC region and final overload fracture area were examined using scanning electron microscopy (SEM) in order to identify the SCC mechanism.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.