Abstract
AbstractBlending with ethylene‐based flexible polymers such as polyethylene (PE) is one of the strategies to toughen poly(lactic acid) (PLA), an inherently brittle biodegradable plastic enjoying growing demands worldwide. Interfacial tension plays a crucial role in blend formulation. Yet several literature reports on the PE/PLA interfacial tension contradict each other, giving ~5 mN/m and ~11 mN/m. In this work, we demonstrate that the PE/PLA interfacial tension is at least 9 mN/m. We use a cocontinuous PE/polystyrene (PS)/PLA ternary blend. Scanning electron microscopy (SEM) revealed complete wetting morphology with PS phase separating PE and PLA phases in the ternary blend. In addition, the complete wetting behavior was maintained at a PS volume fraction as low as 3%. This morphology together with the Harkins equation, indicate that the PE/PLA interfacial tension is higher than 10.5 ± 1.4 mN/m at 180°C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.