Abstract
BaMoO(4):Eu (BEMO) powders were synthesized by the polymeric precursor method (PPM), heat treated at 800 degrees C for 2 h in a heating rate of 5 degrees C/min and characterized by powder X-ray diffraction patterns (XRD), Fourier Transform Infra-Red (FTIR) and Raman spectroscopy, besides room temperature Photoluminescence (PL) measurements. The emission spectra of BEMO samples under excitation of 394 nm present the characteristic Eu(3+) transitions. The relative intensities of the Eu(3+) emissions increase as the concentration of this ion increases from 0.01 to 0.075 mol, but the luminescence is drastically quenched for the Ba(0.855)Eu(0.145)MoO(4) sample. The one exponential decay curves of the Eu(3+ 5)D(0)-->(7)F(2) transition, lambda (exc) = 394 nm and lambda (em) = 614 nm, provided the decay times of around 0.54 ms for all samples. It was observed a broadening of the Bragg reflections and Raman bands when the Eu(+3) concentration increases as a consequence of a more disordered material. The presence of MoO(3) and Eu(2)Mo(2)O(7) as additional phases in the BEMO samples where observed when the Eu(3+) concentration was 14.5 mol%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.