Abstract
It is normally understood as a basic precondition of the etching of swift heavy ion tracks in polymers that both the additives and etching products are soluble in the etchant. If this is not given, the polymer surface may be gradually blocked by the deposition of the insoluble material that acts as a diffusion barrier for the penetration of fresh etchant into the tracks, and therefore the effective track etching speed will gradually be reduced. The etching kinetics is developed for that case, and the theory is compared with first experimental findings. For that purpose we have taken commercial silicone rubber foils as test materials, that were irradiated with GeV heavy ions through a mask at a fluence that corresponds to the onset of track overlapping. After etching with NaOH, the corresponding etching speed was recorded via the reduction of the foil thickness. The etching speed is seen to decrease with exposure time, in parallel to the development of an insoluble surface layer. It is discussed how to prevent that surface blocking, to maintain a high etching speed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.