Abstract

Machinable glass ceramic (MGC) is well known in the micro-electromechanical system and semiconductor industry. Chemical etching is used in this experiment to study the performance of MGC. The etching rate of MGC and its accuracy by indentation method is studied. The categoric parameter applied here is the type of chemical etchant used: hydrochloric (HCl), hydrophosphoric (H3PO4) and hydrobromic (HBr) acids; and, numerical parameters are etching temperature and etching solution. The experimental investigation that was carried out is governed by design of experiment (DoE).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.