Abstract

ESR and ENDOR measurements were performed on undoped poly (p-phenylene vinylene) films obtained by stretching the precursor films under inert gas atmosphere at temperatures between 100°C and 400°C. Weak ESR signals of the spin concentration being roughly 1 spin / 10 6 C 8H 6 unit appeared as the temperature of preparation increased. g value was about 2.003. Spectra showed a clear anisotropy both in g value and line width, where both quantities are larger for the stretch direction. Proton ENDOR signals were also detected and showed larger coupling values for the stretch direction. Observed anisotropy of ESR and ENDOR is qualitatively similar as those observed in stretch oriented polyacetylene, suggesting that the unpaired electrons are π-electron defects on the conjugated molecular chain.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.