Abstract
We report the first deposition of Er/sup 3+/-doped aluminum oxide thin-film optical waveguides by plasma-enhanced chemical vapor deposition (PECVD). The aluminum and erbium precursors used for the deposition of the thin films were trimethyl-aluminum and Er tri-chelate of 2,2,6,6-tetramethylheptane-3,5 dione respectively. The samples show broad, room-temperature photoluminescence at /spl lambda/=1.533 /spl mu/m. The Er/sup 3+/ concentration ranged from 0.01-0.2 at%. The full width half maximum (FWHM) of the Er/sup 3+/ emission spectrum is 55 nm, considerably broader than in silica glass. The radiative lifetime has been measured at 50-mW pump power.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.