Abstract

The Ti deoxidation equilibrium of Fe–Ni, Fe–Cr and Fe–Cr–Ni alloys saturated with ‘Ti3O5’ and Ti2O3 phase was clarified in previous researches. Solubility of Fe, Cr and/or Ni oxides in ‘Ti3O5’ phase equilibrated with liquid Fe–Ni, Fe–Cr and Fe–Cr–Ni alloys at 1823 K to 1923 K were measured by SEM–EDS. It was confirmed that the solubility of Fe, Cr and/or Ni oxide in ‘Ti3O5’ phase at low Ti content increase with decrease of Ti content in alloys. Titanium content that dissolution of Fe, Cr and/or Ni oxide into ‘Ti3O5’ phase becomes apparent increases with increase of Cr and/or Ni content of the alloys. The activity of Ti deoxidation product, ‘Ti3O5’ phase, equilibrated with Fe–Ni, Fe–Cr and Fe–Cr–Ni alloys was also evaluated by Redlich-Kister type polynomial. Equilibrium between Ti and O at low Ti content of those alloys was analyzed using the activity of ‘Ti3O5’ phase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.