Abstract
This paper presents an analytical treatment of equal-frequency surface analysis of a two-dimensional photonic crystal. We first define the equal-frequency surface in terms of plane waves, which can be numerically evaluated. Then one- and two-plane-wave approximations are proposed, which consequently lead to analytical expressions of the equal-frequency surface. The approach presented is well suited to two-dimensional photonic crystals of weak dielectric modulation. For photonic crystals with a large modulation, the approach can be used to gain a general idea of the shape of the bands.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.