Abstract

Initial porous silicon (por‐Si), carbonized porous silicon (por‐Si:C), and carbon‐incorporated porous silicon oxide (por‐SiO2:C) layers are studied by electron paramagnetic resonance (EPR) at T = 10–13 K. Scanning transmission electron microscopy and electron energy loss (EEL) spectroscopy show that por‐Si:C and por‐SiO2:C layers have a highly disordered structure with mixing sp2 and sp3 CC bonds. In the por‐SiO2:C layers, the peak of the oxygen bonded to carbon in the form of hydroxyl groups is found in the EEL spectrum of the C K‐edge region. Low‐intensity signals of Lorentzian lineshape are detected in the EPR spectrum of por‐Si, por‐Si:C, por‐SiO2:C layers. One of them is attributed to the Pb0 defect at the Si/SiO2 interface of nanocrystalline grain and the second to the silicon dangling bonds (SiDB) localized in nanocrystalline Si. The carbonization of por‐Si layers and subsequent oxidation of por‐Si:C gives rise to the appearance of additional EPR signals of high intensity at g = 2.0035(3) in por‐Si:C and at g = 2.0030(3) in por‐SiO2:C, which are assigned to carbon‐related defects (CRD) and carbon clusters, correspondingly. It was found that predominant defect types in por‐Si:C and por‐SiO2:C layers are CRD and carbon clusters, respectively, while the spin concentration of Pb0 interface defects and SiDB is low.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.