Abstract

The effects of acidic and alkaline solutions from wastes leachate on the machine properties of a 2.5 mm thick high density polyethylene (HDPE) geomembranes (GMs) were examined. Smooth/textured HDPE GM specimens were cut into machine direction (MD) and cross machine direction (CMD) which were immersed in the tanks of notched constant tensile load (NCTL) test apparatus containing acidic water (pH=4), alkaline water (pH=8) and incubated at 40 and 60°C respectively. The decline in stress crack resistance of HPDE GMs is evaluated using NCTL tester. In acidic and alkaline conditions, HDPE GMs performed the same stress crack resistance. The increase in temperature and the level of loading shows the decrease in stress crack resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.