This study aims to synthesize Au/TiO2/Na2Ti6O13 composites to reduce the occurrence of recombination and increase photocatalytic activity in phenol degradation. Gold was used due to its high stability and strong surface plasmon resonance (SPR) properties which make it operate effectively in the visible light spectrum. The prepared composites were characterized using XRD, SEM, TEM, FTIR, and DRS. The results showed that the composite consisted of rutile TiO2 with a crystal size of 38–40 nm and Na2Ti6O13 with a crystal size of 25 nm. The gold in the composite has a crystallite size of 16–19 nm along with the percentage of gold added. Morphological analysis shows that the composite has the form of inhomogeneous spherical particles with gold spread among composites with sizes less than 20 nm. FTIR analysis showed the presence of Na–O and Ti–O–Ti bonds in the composite. The best composite was 3% Au/TiO2/Na2Ti6O13 which had high crystallinity, small particle size, and bandgap energy of 2.59 eV. Furthermore, it had an efficiency 205% better than without gold. After that, cost estimation is proposed as a large-scale application. This study describes the total cost, break-even analysis, and payback analysis for the commercialization needs of the designed photocatalytic catalyst.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call