Abstract

AbstractThe addition of rubber powder (RP) to natural rubber (NR) matrix using the dry mixing method leads to uneven distribution and poor interface bonding while the wet mixing method is not feasible due to the hydrophobic nature of the RP surface. To address this issue, we developed a method for producing RP with weakened hydrophobicity on the surface by high‐pressure waterjet and successfully achieved even distribution of the waterjet‐produced rubber powders (WPRPs) in NR and strong interface adhesion between WPRPs and NR by the wet mixing method. The properties of NR/WPRP composites were tested and characterized carefully. When adding 6 phr of 140‐mesh WPRPs in the NR matrix, the tensile strength and elongation at break of the NR/WPRP composites were 30.2 MPa and 627.2%, respectively, which were 4% and 7% higher than NR without WPRPs. Moreover, the anti‐abrasion property of the NR/WPRP composite was also strengthened by the addition of WPRPs. Our findings demonstrate that recycling waste rubber through a reasonable recycling method can not only reduce material waste and alleviate environmental pollution but also enhance the performance of the raw rubber, which offers significant economic benefits.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.