ZnO: Er3+–Yb3+/Gd2O3 core/shell nanoparticles are synthesized via a seeded deposition process with ZnO: Er3+–Yb3+ nanoparticles as seeds and Gd2O3 as shells, respectively. Analyses on phase and structures indicate that the Gd2O3 shell is around 1nm in thickness. Raman signals change with the increase of Gd2O3 shell deposition times, which are the synergistic results of phonon confinement effect and interface strain. Visible up-conversion (UC) emissions are observed in the seed samples, after Gd2O3 surface modification, great enhancement of the UC emissions are observed. The detail is discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.