A series of Sr0.7Ba0.3Nb2O6−δ/x wt. % Ti (x = 1, 3, 5, and 10) composite ceramic thermoelectric materials were prepared, and the mechanism for improving their thermoelectric properties was explored. The experimental results demonstrate that nano-additive titanium powder undergoes oxidation to form TiO2 during sintering. However, under annealing in a reducing atmosphere, oxidation reactions further deplete the lattice oxygen, leading to an increased generation of oxygen vacancies and enhanced carrier concentration, ultimately leading to successful resistivity reduction. The samples consistently exhibit low thermal conductivity values below 2.0 W m−1 K−1 due to crystal defects, complex structure, and phonon scattering at the grain boundaries. The sample doped with 5 wt. %. Ti exhibits the lowest resistivity and highest PF value (409.3 μW/m K2 at 1073 K). Consequently, the figure of merit of Sr0.7Ba0.3Nb2O6−δ with 5 wt. % Ti attains its maximum value of 0.30 at 1073 K, representing a 50% increase compared to that of the undoped sample Sr0.7Ba0.3Nb2O6−δ (0.20 at 1073 K).

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call