Abstract
TiO 2 was reactively sputtered using a combination of a planar and two cylindrical rotatable magnetrons. Using separate argon and oxygen introduction into the system, the planar magnetron was run in the metallic mode while the rotatables were in the oxide mode. In this case, the deposition rate was about three times higher than that obtained running only the two cylindrical rotatable magnetrons in the oxide mode.