Abstract

A pyridobisimidazole unit was introduced into a polymer backbone to obtain an increased doping level, a high number of interacting sites with phosphoric acid and simple processibility. The acid uptake of poly(pyridobisimidazole) (PPI) membrane could reach more than 550% (ADL = 22), resulting in high conductivity (0.23 S·cm−1 at 180 °C). Along with 550% acid uptake, the membrane strength still held 10 MPa, meeting the requirement of Proton Exchange Membrane (PEM). In the Fenton Test, the PPI membrane only lost around 7% weight after 156 h, demonstrating excellent oxidative stability. Besides, PPI possessed thermal stability with decomposition temperature at 570 °C and mechanical stability with a glass transition temperature of 330 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.