The perpendicular magnetic anisotropy (PMA) of the Pd/Co2MnSi(CMS)/Co3O4 and Pd/CMS/Pd/CMS/Co3O4/Pd multilayers has been studied in this paper. The Pd/CMS/ Co3O4 is a “heavy metal (HM)/ferromagnetic (FM) /antiferromagnetic (AFM) oxide” structure that has triple interfacial effects, which is HM/FM, FM/OX and FM/AFM. For Pd (6 nm)/CMS (t nm)/Co3O4 (0.6 nm) /Pd (6 nm) structure, the maximum magnetic anisotropy energy density (Keff) is 0.583 Merg/cm3 at t = 6 nm and the PMA can be maintained with the thickness of the CMS layer in a range of 3.5–8 nm. When the thickness of the Co3O4 layer varied from 0 to 1.3 nm, the multilayer structure also has PMA with 6 nm CMS layer. Inserting a Pd layer in the CMS to form Pd/CMS/Pd/CMS/Co3O4/Pd structure can enhance the PMA and the saturated magnetization. The maximum Keff of the Pd/CMS/Pd/CMS/Co3O4/Pd structure is 0.680 Merg/cm3 by inserting a 0.8 nm Pd layer, which is 15% larger than samples without inserting Pd layer in the CMS. The crystallization quality of Co3O4 relates to the power of sputtering deposition and furthermore affects the flatness of the interface and PMA of the multilayer film.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.