Abstract

Highly (111)-textured ZnxFe3−xO4 thin films were grown by pulsed laser deposition on silicon substrates. The spin and orbital magnetic moments of the ZnxFe3−xO4 thin films have been obtained by X-ray magnetic circular dichroism (XMCD) and sum rule analysis. The total magnetic moments thus extracted are in good agreement with the values obtained by vibrating sample magnetometer. Both the unquenched orbital moment and the ratio of orbital-to-spin moment first increase significantly with increasing Zn substitution at a low concentration range (0≤x≤0.1), and then decrease at a higher concentration (x = 0.3). The underlying site-specific doping mechanisms involved here have been elucidated by detailed analysis of the XMCD of ZnxFe3−xO4 films. Our work demonstrates a practical means to manipulate the spin-orbit coupling in the ZnxFe3−xO4 thin films via Zn impurity doping.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.