Al codoped phosphors were prepared by the alkoxide method, which starts from a hydrolysis of silicon ethoxide and the metal nitrates at low temperature and minimizes the contamination of impurities. An addition of Al ions to is found to increase emission intensity from Sm ion more than an order of magnitude. EXAFS study revealed that local structures around Sm ions in the phosphors with and without dopant are significantly different; in the phosphor Sm atoms are well dispersed at low Sm concentrations and Sm atoms agglomerate at high concentrations, while in the Al codoped phosphor Sm atoms are coordinated by Al through Sm‒O‒Al bonding. This provides a direct structural evidence of the role of the codopant.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.